A 5-year clinical evaluation of ceramic inlays (Cerec) cemented with a dual-cured or chemically cured resin composite luting agent
DOI:
https://doi.org/10.1080/000163598428428Abstract
Sixty-six class-II CAD/CAM-manufactured ceramic inlays (Cerec) were placed in 27 patients. Each patient received at least one inlay luted with a dual-cured resin composite and one inlay luted with a chemically cured resin composite. The inlays were examined 5 years after luting using the California Dental Association (CDA) criteria. Eighty-nine percent of the 66 inlays were rated 'satisfactory'. During the follow-up period replacement was required for 3 inlays because of inlay fractures (4.5%) and 1 inlay because of fracture of the tooth substance (1.5%). All those inlays were luted with the dual-cured resin composite luting agent. Of the remaining 62 inlays the CDA rating 'excellent' was given to 84% for color, 97% for surface, and 81% for anatomic form. 'Excellent' margin integrity was seen in 52% of the dual-cured resin composite luted inlays and in 61% of the chemically cured resin composite luted inlays. No statistically significant (P > 0.05) difference was observed between the two luting agents.
Acta Odontologica Scandinavica publishes original research papers as well as critical reviews relevant to the diagnosis, epidemiology, health service, prevention, aetiology, pathogenesis, pathology, physiology, microbiology, development and treatment of diseases affecting tissues of the oral cavity and associated structures including papers on cause and effect or explanatory/associative relationships for experimental or observational studies.